Product Introduction
The product can conduct electricity through low-temperature sintering, after reaching the critical content, through the seepage effect, tunnel effect and field emission effect, to form a porous continuous structure conductive layer. It provides better flexibility, higher chemical stability, lower sintering temperature and less cost.
Product Features
Particle size uniformity, good dispersion;
Good conductivity, low resistance;
Long-term stable performance, good adhesion, weather resistance.
Usage method
Clean the substrate surface with acetone or ethanol, then dry at 180~200°C for 5~15 minutes.
Uses
Used for making conductive ink, conductive film, printed circuit board and other fields.
Packaging and Storage
Packing: 20kg/barrel.
Storage: in a cool, dry place, frozen storage. After thawing, it can be used for two days at room temperature of 25°C.